Aminoethylated Acrylic Polymer 48.0~50.0(wt%),4000-8000(mPa·s/25℃),MW:1w-3w
A758593-100ML / 100ML
Aminoethylated Acrylic Polymer 48.0~50.0(wt%),4000-8000(mPa·s/25℃),MW:1w-3w
A758593-500ML / 500ML
Aminoethylated Acrylic Polymer 55.0~57.0(wt%),20000-40000(mPa·s/25℃),MW:1w-3w
A758597-100ML / 100ML
Aminoethylated Acrylic Polymer 55.0~57.0(wt%),20000-40000(mPa·s/25℃),MW:1w-3w
A758597-500ML / 500ML
Aminoethylated Acrylic Polymer 33.0~37.0(wt%),400-1500(mPa·s/25℃),MW:10w
A758601-100ML / 100ML
Aminoethylated Acrylic Polymer 33.0~37.0(wt%),400-1500(mPa·s/25℃),MW:10w
A758601-500ML / 500ML
Aminoethylated Acrylic Polymer 29.0~31.0(wt%),<2000(mPa·s/25℃),MW:10w
A758603-100ML / 100ML
Aminoethylated Acrylic Polymer 29.0~31.0(wt%),<2000(mPa·s/25℃),MW:10w
A758603-500ML / 500ML
Anti-Elastase Polyclonal Ab produced in rabbit Protein Concentration: Lot Specific
AB001146-250ΜL / 250ΜL